Magnefast – Polymetallic metal mine

Polymetallic metal mine

Magnefast trial achieved 6 MONTHS service life meeting the current liner objective. The Magnefast liners showed 7 mm of wear in a 50 mm thick ceramic so panels have not been replaced and are expected to eliminate a number of liner…

Request FREE Demo Enquiry

This field is for validation purposes and should be left unchanged.
Name(Required)
Country(Required)

Job Opportunities Enquiry

This field is for validation purposes and should be left unchanged.
Name(Required)
Country(Required)

Request a Quote

This field is for validation purposes and should be left unchanged.
Name(Required)
Country(Required)

Contact Pulley Lagging Popup

This field is for validation purposes and should be left unchanged.
Name(Required)
Country(Required)

Contact Wear Panel Team

This field is for validation purposes and should be left unchanged.
Name(Required)
Country(Required)

Thanks For Requesting
Our Documents

Please provide us quick details before downloading the document.

This field is for validation purposes and should be left unchanged.
Name(Required)